Sign In | Join Free | My futurenowinc.com
China Changzhou Victory Technology Co., Ltd logo
Changzhou Victory Technology Co., Ltd
Active Member

3 Years

Home > Inconel Alloy >

High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate

Changzhou Victory Technology Co., Ltd
Contact Now

High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate

  • 1
  • 2
  • 3

Brand Name : Victory

Model Number : Inconel 718

Certification : ISO9001 ROHS

Place of Origin : China

MOQ : 30 Kg

Price : Negotiable

Payment Terms : L/C, T/T, Western Union, MoneyGram

Supply Ability : 300 tons per month

Delivery Time : 20~40 Days

Packaging Details : Spool Carton box, Coil package with polybag,then in woodencase

Name : High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate

Material : Nickel Chromium Iron

Ni (Min) : 50~55%

Density : 8.24 g/cm3

Melting point : 1260-1320°C

Elongation (≥ %) : 25 %

Thermal conductivity : 15.9 W/m·K

Finishing : Bright,Oxided, acid white

Application : Construction, Industry Oil, piping systems

Yield strength : 550MPa

Tensile strength : 910 MPa

Hardness : ≤ 363 HB

Standard : ASTM, ASME

size : 6~200mm

shape : Round, Square, flat

Contact Now

Inconel 718 Alloy


Inconel 718 is a precipitation hardened nickel-based alloy designed to display exceptionally high yield, tensile and creep-rupture properties at temperatures up to 1300°F (704°C). The age-hardening response of Inconel 718 permits annealing and welding without spontaneous hardening during heating and cooling. Nickel Alloy 718 has excellent weldability when compared to the nickel-base super alloys hardened by aluminum and titanium.

Advantages of Inconel 718 Strips


  • High yield strength
  • Excellent high temperature tensile & creep rupture properties
  • Excellent weldability
  • Does not spontaneously harden
  • Outstanding corrosion resistance

Applications of Inconel 718 Strips


  • Jet engine components
  • Gas turbines
  • Aerospace
  • Plastic injection molded tools
  • High speed airframe parts
  • High temperature bolts & fasteners

Parameter:

Chemical Properties of Inconel 718

Nickel (plus Cobalt) .......................................................50.00-55.00

Chromium......................................................................17.00-21.00

Iron .....................................................................................Balance

Niobium (plus Tantalum)....................................................4.75-5.50

Molybdenum .....................................................................2.80-3.30

Titanium.............................................................................0.65-1.15

Aluminum ..........................................................................0.20-0.80

Cobalt ...............................................................................1.00 max.

Carbon..............................................................................0.08 max.

Manganese .......................................................................0.35 max.

Silicon ...............................................................................0.35 max.

Phosphorus.....................................................................0.015 max.

Sulfur...............................................................................0.015 max.

Boron ..............................................................................0.006 max.

Copper..............................................................................0.30 max

Density 8.19g/cm³ 0.296 lb/in³
Melting point 1260-1336 2437°F

SPECIFICATIONS
Form
ASTM
Rod,bar and wire
B 166
Plate,sheet and strip
B 168, B 906
Seamless pipe and tube
B 167, B 829
Welded pipe
B 517, B775
Fitting
B 366
Billet and bar for reforging
B 472
Forging
B 564

Inconel series

Steel grade
Inconel 600
Inconel 601
Inconel 625
Inconel 718
Inconel 725
Inconel X-750
Corresponding brand
N06600/2.4816/1Cr15Ni75Fe8/NS312/CY40
N06601/2.4851/1Cr23Ni60Fe13AI/NS313
N06625/2.4856/0Cr20Ni65Mo10bN4/NS336
N07718/2.4668/GH4169
N07725
N07750/2.4669/GH4145
Chemical composition%
C≤
0.150
0.100
0.100
0.080
0.030
0.080
Mn≤
1.00
1.00
0.50
0.35
0.35
1.00
P≤
/
/
0.015
0.015
0.015
/
S≤
0.015
0.015
0.015
0.015
0.010
0.010
Si≤
0.50
0.50
0.50
0.35
0.20
0.50
Cr≤
14.0-17.0
21.0-25.0
20.0-23.0
17.0-21.0
19.0-22.5
14.0-17.0
Ni≤
≥72.0
58.0-63.0
≥58.0
55.0-59.0
55.0-59.0
≥70
Mo
/
/
8.0-10.0
2.8-3.3
7.0-9.5
/
Cu
≤0.50
≤1.50
/
≤0.30
/
≤0.50
N
/
/
/
/
/
Nb
/
/
3.15-4.15
4.75-5.50
2.75-4.00
0.70-1.20
other
Fe:6.0-10.0
Al:1.0-1.7
Co:≤1.0Ai:≤0.40Tr:0.40Fe:≤5.0
AI:0.20-0.80Ti:0.65-1.15B≤0.006
Tr:1.0-1.7AI≤0.35
Co:≤1.0 AI:0.4-1.0Tr:0.25-2.75Fe:5.0-9.0

Customize size as below

Shape
Size(mm)
WIre
0.5-7.5
Rod/Bar
8.0-200
Strip
(0.5-2.5)*(5-180)
Tube
custom made
Plate
custom made

contact us

email:victory@dlx-alloy.com

Oem service:
Welcome customized size
We are experience factory for OEM&ODM service

High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plateHigh-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plateHigh-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate


Product Tags:

High strength Nickel-chromium alloy 718

      

Nickel-chromium alloy 718 strip

      

Nickel-chromium alloy 718 foil

      
Wholesale High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate from china suppliers

High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Changzhou Victory Technology Co., Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)